CSWIP 3.1 WELDING DEFECTS

PART 5.png

Key notes:

Undercut

36.png

Excessive reinforcement protection

37.png

The most serious defect – Surface breaking (Lack of Interun fusion on cap)

38.png

Burn though

39.png

Arc strike REPAIRING METHOD

40.png

LOP/LOF

41.png